While FUD and FXD material is used for WoW/WoG less often than WSF (because it is brittle and more expensive), it does have its fans, and it also works well at smaller scales like 1:285. It requires a little bit different handling than WSF -- for instance, it is immersed in hot vegetable oil after printing to remove the support material and -- even though Shapeways does a first pass at washing -- you want to make sure none of that oil is left on the model.
Let's gather all the FUD tips in one sticky thread. If you have wisdom to share on this topic, please follow up here.
You might also find some tips on the Shapeways forums under Finishing Techniques.